Impression Creep Testing Machine

Impression Creep Testing Machine
Impression Creep Testing Machine
Price And Quantity
  • Set/Sets
  • 1
  • Set/Sets
Product Description

Impression Creep Machine

Load Capacity

1 KN

Loading Type

1:10 Lever Arm Cantilever deadweight loading

Indenter

Tungsten Carbide

Indenter dimension

1, 1.5 & 2mm cylindrical (tip dia)

Temperature Range

800 Deg C

Temperature Control

PID, Accuracy +/- 1 Deg C

Vacuum System

Rotary and Diffusion type->6X105 m bar

Max Vacuum range

6X105 m bar

Vacuum Chamber dimension

520mm height, 300mm dia

Specimen dimension

20 Sq X 3mm thick

Sensors used

Load Cell and LVDT

Data Acquisition System01

USB Based NI Lab view data Acquisition system, online plot of Time Vs Depth of Indentation and Strain

Trade Information
  • 5 Per Month
  • 2 Week
    Contact Us

    #19/1-2, Lakshmi Nivasa, 1st Main Road, Manivilas Garden, Vrushabhavathi Nagar, Bengaluru, Karnataka, 560079, India
    Phone :+918035063303